Aerospace series - Zinc-Nickel (12 %-16 % Ni) plating of steels with specified tensile strength . 1 450 MPa, copper alloys, nickel alloys and aluminium alloys for parts and fasteners
NORM herausgegeben am 1.7.2015
Bezeichnung normen: ČSN EN 4826
Zeichen: 318216
Katalog-Nummer: 97270
Ausgabedatum normen: 1.7.2015
Zahl der Seiten: 20
Gewicht ca.: 60 g (0.13 Pfund)
Land: Tschechische technische Norm
Kategorie: Technische Normen ČSN
This European Standard specifies the plating of a Zinc-Nickel (12 % to 16 %) alloy on mechanical parts and fasteners in steels (Rm <= 1 450 MPa), stainless steels (Rm <= 1 450 MPa), copper alloys, nickel alloys and aluminium alloys (not applicable for electrical components), as well as the passivation and lubricant finishing that can be associated to them. The Zinc-Nickel process is an electrolytic plating process under controlled current allowing to deposit a Zinc-Nickel layer from, most often, an alkaline electrolyte. Alkaline Zinc-Nickel is only considered in this standard.
The purpose of this standard is to give technical and quality requirements of Zinc-Nickel plating. It doesn´t give complete in-house process instructions, these shall be given in the manufacturers detailed process instructions