Wir benötigen Ihre Einwilligung zur Verwendung der einzelnen Daten, damit Sie unter anderem Informationen zu Ihren Interessen einsehen können. Klicken Sie auf "OK", um Ihre Zustimmung zu erteilen.
Standard Specification for Nickel Rod and Bar (Includes all amendments And changes 10/8/2014).
Automatische name übersetzung:
Standard-Spezifikation für Nickel und Stab
NORM herausgegeben am 1.10.2009
Bezeichnung normen: ASTM B160-05(2009)e1
Anmerkung: UNGÜLTIG
Ausgabedatum normen: 1.10.2009
SKU: NS-5521
Zahl der Seiten: 6
Gewicht ca.: 18 g (0.04 Pfund)
Land: Amerikanische technische Norm
Kategorie: Technische Normen ASTM
Keywords:
bar, rod, N02200, N02201, N02211, Nickel--specifications, Nickel alloy rod/bar/wire--specifications, UNS N02200 (commercially pure Ni alloy, Nickel 200), UNS N02201 (commercially pure Ni alloy, Nickel 201), ICS Number Code 2211, 77.150.40 (Nickel and chromium products)
1. Scope | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
1.1 This specification covers nickel (UNS N02200)*, low carbon nickel (UNS N02201)*, and solution strengthened nickel (UNS N02211) in the form of hot-worked and cold-worked rod and bar in the conditions shown in Table 1. 1.2 The values stated in inch-pound units are to be regarded as standard. The values given in parentheses are mathematical conversions to SI units that are provided for information only and are not considered standard. 1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to become familiar with all hazards including those identified in the appropriate Material Safety Data Sheet (MSDS) for this product/material as provided by the manufacturer, to establish appropriate safety and health practices, and determine the applicability of regulatory limitations prior to use. TABLE 1 Mechanical Properties
A See 12.2. B Not applicable to diameters or cross sections under 3/32 in. (2.4 mm). C For hot-worked flats 5/16 in. (7.9 mm) and under in thickness the elongation shall be 25%, min. D Hardness B45 to B80, or equivalent. E Hardness B45 to B70 or equivalent. F Forging quality is furnished to chemical requirements and surface inspection only. No tensile properties are required. |
||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
2. Referenced Documents | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
|
Wollen Sie sich sicher sein, dass Sie nur die gültigen technischen Normen verwenden?
Wir bieten Ihnen eine Lösung, die Ihnen eine Monatsübersicht über die Aktualität der von Ihnen angewandten Normen sicher stellt.
Brauchen Sie mehr Informationen? Sehen Sie sich diese Seite an.
Letzte Aktualisierung: 2024-05-07 (Zahl der Positionen: 2 897 585)
© Copyright 2024 NORMSERVIS s.r.o.